  1. KappaTinning™ Compound - Case of 4 x 12.5 lb pails
    KappaTinning™ Compound - Case of 4 x 12 lb. pails
    $1,250.00

    KappaTinning™ Compound is a dry mixture of pure powdered Tin and flux specifically designed for pre-tinning Cast Iron, Steel, Bronze, and Copper bearing shells. A one-pound container has about twice as much Tin and goes further than other tinning compounds. Case of 4 - 12.5 lb pails.

    VIEW PRODUCT
  2. KappaTinning™ Compound - 12.5 lb pail
    KappaTinning™ Compound - 12 lb. pail
    $438.00
    KappaTinning™ Compound is a dry mixture of pure powdered Tin and flux specifically designed for pre-tinning Cast Iron, Steel, Bronze, and Copper bearing shells. A one-pound container has about twice as much Tin and goes further than other tinning compounds. 12.5 lb pail. VIEW PRODUCT
  3. KappaTinning™ Compound - 1 lb jar
    KappaTinning™ Compound - 1 lb jar
    $38.50
    KappaTinning™ Compound is a dry mixture of pure powdered Tin and flux specifically designed for pre-tinning Cast Iron, Steel, Bronze, and Copper bearing shells. A one-pound container has about twice as much Tin and goes further than other tinning compounds. 1 lb in a plastic jar. VIEW PRODUCT

3 Items

View as Grid List
per page
Set Descending Direction

KappaTinning™ Compound  is a dry mixture of pure powdered Tin and flux specifically designed for pre-tinning Cast Iron, Steel, Bronze, and Copper bearing shells. A one-pound container has about twice as much Tin and goes further than other tinning compounds currently on the market.

 

Applications

  • Provides a uniform strong bond between the Babbitt alloy and the bearing shell surface on:
  • Brass
  • Bronze
  • Steel
  • Cast Iron
  • Paired with Kapp CopperBond™ Flux

Properties

Technical Data

Appearance:

Light, Silvery Gray Powder

Water Solubility:

Approximately 50%

Odor:

None

Density:

5.0 g/cm (0.1794lbs/in3)

%Volatile:

0%

pH (in 10% aqueous solution):

1.5

Product Variants

  • 1lb. (0.5 kg) plastic jars
  • 12.5 lb. (5.7 kg) plastic tubs
  • Case of 12.5 lb. (5.7 kg)  plastic tubs (4 tubs) = 50 lbs (22.7kg)

Also Order

 

Click here for KappaTinning™ Compound Technical Data Sheet

 

Click here for KappaTinning™ Compound Safety Data Sheet

 

Instructions

1.     Pre-clean and degrease the bearing surface prior to tinning. Particular attention should be given to Cast Iron bearings to remove silica surface skins, graphite, and other residues that may impair adhesion. Kapp CopperBond™ Flux can be used to draw the impurities out of the bearing surface.

2.     Pre-heat the bearing shell to approximately 500-550°F (260-288°C); (excessive heat may cause flux charring and premature Tin oxidation).

3.     Sprinkle KappaTinning™ Compound on the bearing surface and vigorously wipe with a stainless steel wire brush or steel wool to yield a smooth, well-tinned surface to which Babbitt will readily bond.

4.     Flux residues are completely water-soluble and should be washed off promptly prior to Babbitt application.

Storage

Keep container lid tightly closed when not in use. Store in a cool, dry place away from heat. Shelf life of this product is 1½ years if container is unopened.

 

Safety

While KappaTinning™ Compound is not considered toxic, upon heating it will generate decomposition and reaction vapors. These vapors should be adequately exhausted during heating. Consult SDS for additional safety information.

 